Question: Swelling of the SU-8 during exposure 

Forum: SU-8 Photoresist Discussion Forum
Date: 2004, Dec 02
From: Carson <svetleis@yahoo.fr>

Hello All,

I am using the SU-8 2035 for making film thicknesses of 50 microns.

I am proceeding with the soft and hard bake in a normal way. After my exposure I can see clearly that around the structure I have considerable swelling of my polymer, around 100% of my original thickness. SOmetimes the polymer sticks well, sometimes it delaminates from its region Also, the structure I expose is somewhat always minored in dimensions in comparison of my original mask.

Has someone ever encountered this problem?

Is it due to a wrong exposure time (I am using a UV source , 365 nm), 7 to 9 seconds?

Is it due to a bad curing? maybe should be longer to reduce stress?

Many thanks for your help CArson

[ Next-in-Thread ]  [ Next Message ] 

Messages Inline: [ 1 ]  [ All ]  Outline: [ 1 ]  [ 2 ]  [ 3 ] 

[ Add Message ]  to: "Swelling of the SU-8 during exposure"

[ Register ]  [ Subscribe ]  [ Admin Mode ] 
[ Show Frames ]  [ Search ]  [ Help for Discussion Forum 1.10EW ] 

Terms of Use | Privacy Policy | Site Map | Related MEMS Links | Search this Site

Copyright Sporian Microsystems