Hi all,
I have a question about the omnicoat for the su8. I use glass slide as my substrate. If I want to use omnicoat, need I spin a layer of HMDS before I spin the omnicoat. Another question is are there some persons who have experience in the su8 bonding. I fabricate channel with su8-50, and then spin su8-2 on another glass slide and then bond the two slides. But I failed several times, doesn't anybody can give me some advice. Thank you very much! huinan
|